Dry sliding wear behaviour of thixoformed AL-5.7SI-2CU-0.3MG aluminium alloy/
Saved in:
Main Author: | |
---|---|
Format: | Thesis Book |
Language: | English |
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
LEADER | 01298nam a2200313 a 4500 | ||
---|---|---|---|
008 | 200723s2019 my 000 0 eng d | ||
040 | |a UKM |e rda | ||
090 | |a TA483 |b .A2364 2019 3 tesis | ||
100 | 1 | |a Abdelgnel, Mnel A.H. |e author. | |
245 | 1 | 0 | |a Dry sliding wear behaviour of thixoformed AL-5.7SI-2CU-0.3MG aluminium alloy/ |c Mnel A H Abdelgnel. |
264 | 0 | |a |c 2019. | |
300 | |a xxi, 216 pages : |b illustrations ; |c 30 cm.+ \e 1 computer optical discs (4 3/4 in.). | ||
336 | |a text |2 rdacontent | ||
337 | |a unmediated |2 rdamedia | ||
338 | |a volume |2 rdacarrier | ||
502 | |a Thesis (Ph.D.) - Universiti Kebangsaan Malaysia, 2019. | ||
504 | |a Reference : page 194-216. | ||
593 | |a Cd yang disertakan adalah duplikasi kepada tesis bercetak dan tidak boleh dirujuk/dipinjam. | ||
610 | 2 | 0 | |a Universiti Kebangsaan Malaysia |x Dissertations. |
650 | 0 | |a Alloys. | |
650 | 0 | |a Microstructure. | |
650 | 0 | |a Aluminum. | |
650 | 0 | |a Dissertations, Academic |z Malaysia. | |
907 | |a .b16819263 |b 24-11-21 |c 23-07-20 | ||
998 | |a l0013 |b 23-07-20 |c m |d x |e - |f eng |g my |h 0 | ||
949 | |o 101002636 (3) | ||
990 | |a SMY/MKN | ||
991 | |a Fakulti Kejuruteraan dan Alam Bina | ||
945 | |a TA483.A2364A 2019 3 tesis |g 1 |i 00002236292 |j 0 |l l0013 |o - |p MYR0.00 |q - |r - |s - |t 3 |u 0 |v 0 |w 0 |x 0 |y .i21473286 |z 24-11-21 |