Fabrication and characterisation of aluminium doped silica fibre preform
This thesis describes the fabrication and characterisation of alumina-doped silica fiber preforms by the modified chemical vapour deposition (MCVD) method coupled with solution doping technique. The silica soot deposited at 1800°C was examined by scanning electron microscopy (SEM) and gas adsorption...
Saved in:
Main Author: | Salah Abdullah, Salah Mohammed |
---|---|
Format: | Thesis |
Published: |
2014
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Mechanical strength of as-compacted aluminium alloy waste chips
by: Khalid, Siti Nor Azila
Published: (2013) -
Copper deposition on polyimide by reduction and chemical vapour deposition /
by: Chen, Lina
Published: (2001) -
The effect of vortex well thickness on microstructure and mechanical properties of aluminium LM6
by: Hehsan, Haffidzudin
Published: (2013) -
Hot-wire plasma enhanced chemical vapour deposition system for preparation of silicon carbide thin films /
by: Aniszawati Azis
Published: (2012) -
Fabrication and characterization of polymeric and nanostructured carbon nitride thin films : a simple difference in electrode distance /
by: Richard Ritikos
Published: (2011)