The paper properties of Kenaf from APMP pulping process using RSM / Syaiedeen Awang Rani

In this particular research, the kenaf stalk variety of V 36 has been pulped using Alkaline Peroxide Mechanical Pulping (APMP). Three pulping parameters were studied such as the percentages of hydrogen peroxide, sodium hydroxide and soaking time. The regression equation was obtained to determin...

Full description

Saved in:
Bibliographic Details
Main Author: Awang Rani, Syaiedeen
Format: Thesis
Language:English
Published: 2020
Subjects:
Online Access:https://ir.uitm.edu.my/id/eprint/60035/1/60035.pdf
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In this particular research, the kenaf stalk variety of V 36 has been pulped using Alkaline Peroxide Mechanical Pulping (APMP). Three pulping parameters were studied such as the percentages of hydrogen peroxide, sodium hydroxide and soaking time. The regression equation was obtained to determine the fitness of the quadratic model. The range of the sodium hydroxide (NaOH) used was between 6% to 12% and the hydrogen peroxide (H2O2) in 30% concentration was in range 5% to 10%. The soaking time was set between 45 and 90 minutes. The temperature was at 70 oC constant at each experimental runs. The design of experiment (DOE) was analyzed and determined to produce 17 experimental design runs. The statistical analysis and experimental runs was done by using Response Surface Methodology (RSM) and by applying Design Expert 6. The paper properties studied were physical properties such as tensile, tear and burst strength. The optical properties were brightness and opacity. The optimum condition for the pulping parameter that has been obtained was: H2O2 at 8.33%, NaOH at 6.05% and soaking time at 55.75 minutes. The actual responses produced were at 25.05Nm2/g for tensile index17.32mNm2/g for the tear index, and 3.6433kPam2/g for the burst index, 61.49% for the brightness percentages and 89.7617% for the opacity percentages.