The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite
Hybrid kenaf-glass fiber unsaturated polyester composite was prepared by hand lay-up technique. The kenaf was used in a fiber mat form. The effect of layer number of hybrid kenaf-glass fiber unsaturated polyester composite on mechanical properties and dimensional stability were studied. The effec...
Saved in:
Main Author: | |
---|---|
Format: | Thesis |
Language: | English |
Subjects: | |
Online Access: | http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/1/Page%201-24.pdf http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/2/Full%20text.pdf |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my-unimap-41299 |
---|---|
record_format |
uketd_dc |
spelling |
my-unimap-412992016-04-13T06:49:58Z The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite Nor Azian, Mohamad Dr Rozyanty Rahman Hybrid kenaf-glass fiber unsaturated polyester composite was prepared by hand lay-up technique. The kenaf was used in a fiber mat form. The effect of layer number of hybrid kenaf-glass fiber unsaturated polyester composite on mechanical properties and dimensional stability were studied. The effect of layer number of hybrid kenaf-glass fiber unsaturated polyester composite has shown good interfacial adhesion between matrix and fiber reinforced composite thus, increasing the tensile and flexural strength of hybrid kenaf-glass fiber unsaturated polyester composite. Results show that four layer of hybrid kenaf-glass fiber unsaturated polyester composite laminates have the highest tensile strength i.e. 52.665 MPa while highest flexural strength was obtained in two layer of hybrid kenaf-glass fiber unsaturated polyester composite laminate i.e. 92.77 MPa. Three layer of hybrid kenaf-glass fiber unsaturated polyester composite laminate have showed the highest thermal stability at high temperature 452.34˚C with ratio glass fiber to kenaf 2:1. Highest dimensional stability in ethanol solution for 1800 minutes with average of 2 % changes was shown in two layer of hybrid kenaf-glass fiber polyester composite laminate. Universiti Malaysia Perlis (UniMAP) 2014-03 Thesis en http://dspace.unimap.edu.my:80/xmlui/handle/123456789/41299 http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/1/Page%201-24.pdf 6a1141d13f37adb9ebd6677d6e99b77f http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/2/Full%20text.pdf 7405ee0ef55571229bec32f2553f6462 http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/3/license.txt 8a4605be74aa9ea9d79846c1fba20a33 Polyester composite Hybrid kenaf-glass fiber Kenaf Composites School of Materials Engineering |
institution |
Universiti Malaysia Perlis |
collection |
UniMAP Institutional Repository |
language |
English |
advisor |
Dr Rozyanty Rahman |
topic |
Polyester composite Hybrid kenaf-glass fiber Kenaf Composites |
spellingShingle |
Polyester composite Hybrid kenaf-glass fiber Kenaf Composites Nor Azian, Mohamad The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
description |
Hybrid kenaf-glass fiber unsaturated polyester composite was prepared by hand
lay-up technique. The kenaf was used in a fiber mat form. The effect of layer number of
hybrid kenaf-glass fiber unsaturated polyester composite on mechanical properties and
dimensional stability were studied. The effect of layer number of hybrid kenaf-glass
fiber unsaturated polyester composite has shown good interfacial adhesion between
matrix and fiber reinforced composite thus, increasing the tensile and flexural strength of
hybrid kenaf-glass fiber unsaturated polyester composite. Results show that four layer of
hybrid kenaf-glass fiber unsaturated polyester composite laminates have the highest
tensile strength i.e. 52.665 MPa while highest flexural strength was obtained in two layer
of hybrid kenaf-glass fiber unsaturated polyester composite laminate i.e. 92.77 MPa.
Three layer of hybrid kenaf-glass fiber unsaturated polyester composite laminate have
showed the highest thermal stability at high temperature 452.34˚C with ratio glass fiber
to kenaf 2:1. Highest dimensional stability in ethanol solution for 1800 minutes with
average of 2 % changes was shown in two layer of hybrid kenaf-glass fiber polyester
composite laminate. |
format |
Thesis |
author |
Nor Azian, Mohamad |
author_facet |
Nor Azian, Mohamad |
author_sort |
Nor Azian, Mohamad |
title |
The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
title_short |
The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
title_full |
The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
title_fullStr |
The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
title_full_unstemmed |
The effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
title_sort |
effect of layer number on mechanical properties and dimensional stability of hybrid kenaf-glass fiber unsaturated polyester composite |
granting_institution |
Universiti Malaysia Perlis (UniMAP) |
granting_department |
School of Materials Engineering |
url |
http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/1/Page%201-24.pdf http://dspace.unimap.edu.my:80/xmlui/bitstream/123456789/41299/2/Full%20text.pdf |
_version_ |
1747836814255718400 |