Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.

Throughout this investigation, paddles from the SIMEM concrete mixer plant were selected as the subject for this wear analysis. The numbers of paddles studied are twenty. The performance and wear progress of the paddles were monitored periodically. In this project, six types of hard facing alloy...

全面介绍

Saved in:
书目详细资料
主要作者: Chiong, Kung Kwong
格式: Thesis
语言:English
English
出版: 2003
主题:
在线阅读:http://psasir.upm.edu.my/id/eprint/12205/1/FK_2003_46.pdf
标签: 添加标签
没有标签, 成为第一个标记此记录!
id my-upm-ir.12205
record_format uketd_dc
spelling my-upm-ir.122052024-07-04T08:30:55Z Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces. 2003-08 Chiong, Kung Kwong Throughout this investigation, paddles from the SIMEM concrete mixer plant were selected as the subject for this wear analysis. The numbers of paddles studied are twenty. The performance and wear progress of the paddles were monitored periodically. In this project, six types of hard facing alloy were welded onto the same base metal, cast manganese materials. Hard surfacing is an effective method of modifying the surface properties without changing the whole materials of the paddle. These hard-facing alloys (severe wear resistant and moderate impact resistance characteristics) were welded onto the surfaces and edges of each paddle respectively (each hard facing alloys on three paddles). These welds were as cross lines of 20 mm apart all over the top surface of each paddle and full weld on the front side edges for maximum wear protection. Each weld bead deposited is 3 to 4mm thick and 5 to 6mm wide.Two paddles were selected without any hard facing protective layers in this analysis as a reference purpose. Hard facing alloys used in this research are high Chromium high Carbon alloys (Paddles AI, A2, A3, A4, A5, A6, A7, A9, A11), Complex Chromium Carbide alloys with Boron (Paddles B1 , B2, B3, B4, B5 and B6) and Tungsten Carbide material on paddle B7, B9 and B11. The main parameters measured were the side dimensions loss, thickness loss, volume loss and mass loss. Data collection was collected on a monthly basis in order to obtained higher accuracy. Two sets of paddles were used for each type of hard facing. As one set is in the measuring stage, the next set is fitted in the concrete mixer. Concrete - Mixing Concrete mixers Paddle-wheels 2003-08 Thesis http://psasir.upm.edu.my/id/eprint/12205/ http://psasir.upm.edu.my/id/eprint/12205/1/FK_2003_46.pdf text en public masters Universiti Putra Malaysia Concrete - Mixing Concrete mixers Paddle-wheels Faculty of Engineering Khalid, Yousif A. English
institution Universiti Putra Malaysia
collection PSAS Institutional Repository
language English
English
advisor Khalid, Yousif A.
topic Concrete - Mixing
Concrete mixers
Paddle-wheels
spellingShingle Concrete - Mixing
Concrete mixers
Paddle-wheels
Chiong, Kung Kwong
Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
description Throughout this investigation, paddles from the SIMEM concrete mixer plant were selected as the subject for this wear analysis. The numbers of paddles studied are twenty. The performance and wear progress of the paddles were monitored periodically. In this project, six types of hard facing alloy were welded onto the same base metal, cast manganese materials. Hard surfacing is an effective method of modifying the surface properties without changing the whole materials of the paddle. These hard-facing alloys (severe wear resistant and moderate impact resistance characteristics) were welded onto the surfaces and edges of each paddle respectively (each hard facing alloys on three paddles). These welds were as cross lines of 20 mm apart all over the top surface of each paddle and full weld on the front side edges for maximum wear protection. Each weld bead deposited is 3 to 4mm thick and 5 to 6mm wide.Two paddles were selected without any hard facing protective layers in this analysis as a reference purpose. Hard facing alloys used in this research are high Chromium high Carbon alloys (Paddles AI, A2, A3, A4, A5, A6, A7, A9, A11), Complex Chromium Carbide alloys with Boron (Paddles B1 , B2, B3, B4, B5 and B6) and Tungsten Carbide material on paddle B7, B9 and B11. The main parameters measured were the side dimensions loss, thickness loss, volume loss and mass loss. Data collection was collected on a monthly basis in order to obtained higher accuracy. Two sets of paddles were used for each type of hard facing. As one set is in the measuring stage, the next set is fitted in the concrete mixer.
format Thesis
qualification_level Master's degree
author Chiong, Kung Kwong
author_facet Chiong, Kung Kwong
author_sort Chiong, Kung Kwong
title Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
title_short Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
title_full Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
title_fullStr Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
title_full_unstemmed Wear Performance Of Concrete Mixture Paddles With Hardened Surfaces.
title_sort wear performance of concrete mixture paddles with hardened surfaces.
granting_institution Universiti Putra Malaysia
granting_department Faculty of Engineering
publishDate 2003
url http://psasir.upm.edu.my/id/eprint/12205/1/FK_2003_46.pdf