Effects Of Current Density, Etching Time And Hydrofluoric Acid Concentration On The Formation And Morphology Of Highly Doped N-Type Porous Silicon
Highly doped n-type porous silicons (PS) were prepared via electrochemical etching. The effect of current density (50 – 300 mA cm-2), etching time (30 – 300 s) and HF concentration (9.2 – 49.0% (v/v)) on the morphology, pore diameter, porosity, surface roughness and electrical properties of the PS w...
Saved in:
Main Author: | Yaakob, Suriani Haji |
---|---|
Format: | Thesis |
Language: | English |
Published: |
2011
|
Subjects: | |
Online Access: | http://eprints.usm.my/42764/1/SURIANI_HAJI_YAAKOB.pdf |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Black Silicon Fabricated By Aluminium-Assisted Chemical Etching For Solar Cells
by: Uddin, Shahnawaz
Published: (2023) -
Surface morphology, optical and electrical properties of porous silicon produced by chemical etching
by: Tham, Dwight Jern Ee -
Investigation of etching mechanism and hillock formation on silicon etched using tmah /
by: Luo, Ping
Published: (2001) -
Investigation of pyramid formation on Tmah etched silicon /
by: Bai, Yang
Published: (2000) -
Development Of N-Type Spin-On Dopant For Silicon Devices
by: Ahmad Kamil, Suraya
Published: (2009)