LiNbO3 and Nd3+ doped LiNbO3 crystals have successfully been grown by using Czochralski (CZ) method. Their crystallinity has been confirmed using X-ray diffraction (XRD) technique and the result has been used to determine the lattice parameters. The density of the crystals is measured using Archimed...

Full description

Saved in:
Bibliographic Details
Main Author: Mohammad Naim, Norshafadzila
Format: Thesis
Language:English
Published: 2012
Subjects:
Online Access:http://eprints.utm.my/id/eprint/33382/5/NorshafadzilaMohammadNaimMFS2012.pdf
Tags: Add Tag
No Tags, Be the first to tag this record!
id my-utm-ep.33382
record_format uketd_dc
spelling my-utm-ep.333822021-05-27T05:20:02Z Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method 2012-03 Mohammad Naim, Norshafadzila QD Chemistry LiNbO3 and Nd3+ doped LiNbO3 crystals have successfully been grown by using Czochralski (CZ) method. Their crystallinity has been confirmed using X-ray diffraction (XRD) technique and the result has been used to determine the lattice parameters. The density of the crystals is measured using Archimedes principle while the transmission spectra are obtained using Fourier Transform Infrared Spectroscopy (FTIR). Their absorption characteristic is determined using Ultra Violet-Visible (UV-Vis) Spectroscopy. From the X-ray diffraction spectra, it is found that the samples exhibit single phase congruent composition and the lattice parameter of a and c are in the range of 5.1423Å – 5.1711Å and 13.8482Å – 13.9258Å, respectively. The crystals density is found to be ranging from 4.637 g cm-3 – 4.649 g cm-3 and it is in the increasing trend with respect to Nd3+ content. The crystals present a broad OH- absorption band located at approximately 3486 cm-1. It is observed that the addition small amount of Nd3+ ion into the system has small effect on the absorption band position and does not change the crystal structure. It is also found that the increasing amount of Nd3+ content caused the optical band gap Eg to increase from 3.72 eV to 3.80 eV and 3.48 eV to 3.60 eV for direct transition allowed and forbidden, respectively. Meanwhile, the Eg for indirect transition allowed and forbidden are about 3.36 eV – 3.52 eV and 3.15 eV – 3.36 eV, respectively. The Urbach energy, ∆E is found to be in the range of 0.30 eV – 0.45 eV and increases with Nd3+ content. Meanwhile, the addition of Nd3+ ion caused the refractive index to decrease from 2.480 to 2.008 and increase the Judd-Ofelt intensity parameters, from 0.3006×10-19 to 1.8490×10-19 for Ω2, 0.9213×10-19 to 4.4042×10-19 for Ω4 and 0.9511×10-19 to 6.2420×10-19 for Ω6. 2012-03 Thesis http://eprints.utm.my/id/eprint/33382/ http://eprints.utm.my/id/eprint/33382/5/NorshafadzilaMohammadNaimMFS2012.pdf application/pdf en public masters Universiti Teknologi Malaysia, Faculty of Science Faculty of Science
institution Universiti Teknologi Malaysia
collection UTM Institutional Repository
language English
topic QD Chemistry
spellingShingle QD Chemistry
Mohammad Naim, Norshafadzila
Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
description LiNbO3 and Nd3+ doped LiNbO3 crystals have successfully been grown by using Czochralski (CZ) method. Their crystallinity has been confirmed using X-ray diffraction (XRD) technique and the result has been used to determine the lattice parameters. The density of the crystals is measured using Archimedes principle while the transmission spectra are obtained using Fourier Transform Infrared Spectroscopy (FTIR). Their absorption characteristic is determined using Ultra Violet-Visible (UV-Vis) Spectroscopy. From the X-ray diffraction spectra, it is found that the samples exhibit single phase congruent composition and the lattice parameter of a and c are in the range of 5.1423Å – 5.1711Å and 13.8482Å – 13.9258Å, respectively. The crystals density is found to be ranging from 4.637 g cm-3 – 4.649 g cm-3 and it is in the increasing trend with respect to Nd3+ content. The crystals present a broad OH- absorption band located at approximately 3486 cm-1. It is observed that the addition small amount of Nd3+ ion into the system has small effect on the absorption band position and does not change the crystal structure. It is also found that the increasing amount of Nd3+ content caused the optical band gap Eg to increase from 3.72 eV to 3.80 eV and 3.48 eV to 3.60 eV for direct transition allowed and forbidden, respectively. Meanwhile, the Eg for indirect transition allowed and forbidden are about 3.36 eV – 3.52 eV and 3.15 eV – 3.36 eV, respectively. The Urbach energy, ∆E is found to be in the range of 0.30 eV – 0.45 eV and increases with Nd3+ content. Meanwhile, the addition of Nd3+ ion caused the refractive index to decrease from 2.480 to 2.008 and increase the Judd-Ofelt intensity parameters, from 0.3006×10-19 to 1.8490×10-19 for Ω2, 0.9213×10-19 to 4.4042×10-19 for Ω4 and 0.9511×10-19 to 6.2420×10-19 for Ω6.
format Thesis
qualification_level Master's degree
author Mohammad Naim, Norshafadzila
author_facet Mohammad Naim, Norshafadzila
author_sort Mohammad Naim, Norshafadzila
title Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
title_short Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
title_full Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
title_fullStr Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
title_full_unstemmed Optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
title_sort optical properties of neodymium doped lithium niobate single crystals grown by czochralski method
granting_institution Universiti Teknologi Malaysia, Faculty of Science
granting_department Faculty of Science
publishDate 2012
url http://eprints.utm.my/id/eprint/33382/5/NorshafadzilaMohammadNaimMFS2012.pdf
_version_ 1747816147656376320