The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy

Aluminum alloy castings are being used progressively more in safety-critical applications in the automotive and aerospace industries. During the production of aluminum ingots and castings, the surface oxide on the liquid is folded in to produce crack-like defects (bifilms), porosities that are...

全面介紹

Saved in:
書目詳細資料
主要作者: Subhi, Zaid Ali
格式: Thesis
語言:English
出版: 2012
主題:
在線閱讀:http://eprints.uthm.edu.my/2472/1/24p%20ZAID%20ALI%20SUBHI.pdf
標簽: 添加標簽
沒有標簽, 成為第一個標記此記錄!
id my-uthm-ep.2472
record_format uketd_dc
spelling my-uthm-ep.24722022-02-03T01:49:52Z The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy 2012-02 Subhi, Zaid Ali TS Manufactures TS200-770 Metal manufactures. Metalworking Aluminum alloy castings are being used progressively more in safety-critical applications in the automotive and aerospace industries. During the production of aluminum ingots and castings, the surface oxide on the liquid is folded in to produce crack-like defects (bifilms), porosities that are extremely thin and tiny or big, but can be extremely extensive, and so constitute seriously detrimental defects. To produce castings of sufficient quality, it is, therefore, important to understand the mechanisms of the formation of defects in aluminum melt flow through the gating system. Gating system design is an essential element in casting process which affects significantly the molten metal flow behavior, heat transfer and solidification of the melt. The good quality casting product could be achieved by using an optimum gating design. This study has employed Vortex gate design of LM25 (Al—7Si-0.3Mg) thin section casting to determine the effect of Vortex and Conventional gate design on mechanical properties and porosity distribution pattern. Numerical simulation by ADESTEFAN v.10 package was used to identify the molten metal flow behavior in the mold cavity which is physically could not be detected by unaided eye. The X-Ray Radiography test used to examine in general the distribution of defects in thin casted part. 3-Point bending test was applied to measure the flexural strength of the casted alloy material. The scattering of flexural strength has been quantified by Weibull statistics approach. The microstructure inspection was observed using both, the optical microscope micrographs and scanning electron machine (SEM) tests. Numerical simulation results showed a smooth and non turbulent flow of the Vortex gate design. The liquid metal in vortex entering the mould cavity is helped by gravity for a good free surface condition during filling, reducing the danger of entrapment of any free surface film. Furthermore, experimental results showed that casting product with vortex gate leads to excellent improvement of average flexural strength and reduction of porosity and cracks defects relying on the feature of swirled flow inside the vortex gate. The ‘virtual’ experiment using a computational modeling package and the ‘physical’ experiment were found to be in reasonable agreement. 377$ 3(53867$.$$1�781.8�781�$0,1$+ 2012-02 Thesis http://eprints.uthm.edu.my/2472/ http://eprints.uthm.edu.my/2472/1/24p%20ZAID%20ALI%20SUBHI.pdf text en public mphil masters Universiti Tun Hussein Onn Malaysia Fakulti Kejuruteraan Mekanikal dan Pembuatan
institution Universiti Tun Hussein Onn Malaysia
collection UTHM Institutional Repository
language English
topic TS Manufactures
TS Manufactures
spellingShingle TS Manufactures
TS Manufactures
Subhi, Zaid Ali
The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
description Aluminum alloy castings are being used progressively more in safety-critical applications in the automotive and aerospace industries. During the production of aluminum ingots and castings, the surface oxide on the liquid is folded in to produce crack-like defects (bifilms), porosities that are extremely thin and tiny or big, but can be extremely extensive, and so constitute seriously detrimental defects. To produce castings of sufficient quality, it is, therefore, important to understand the mechanisms of the formation of defects in aluminum melt flow through the gating system. Gating system design is an essential element in casting process which affects significantly the molten metal flow behavior, heat transfer and solidification of the melt. The good quality casting product could be achieved by using an optimum gating design. This study has employed Vortex gate design of LM25 (Al—7Si-0.3Mg) thin section casting to determine the effect of Vortex and Conventional gate design on mechanical properties and porosity distribution pattern. Numerical simulation by ADESTEFAN v.10 package was used to identify the molten metal flow behavior in the mold cavity which is physically could not be detected by unaided eye. The X-Ray Radiography test used to examine in general the distribution of defects in thin casted part. 3-Point bending test was applied to measure the flexural strength of the casted alloy material. The scattering of flexural strength has been quantified by Weibull statistics approach. The microstructure inspection was observed using both, the optical microscope micrographs and scanning electron machine (SEM) tests. Numerical simulation results showed a smooth and non turbulent flow of the Vortex gate design. The liquid metal in vortex entering the mould cavity is helped by gravity for a good free surface condition during filling, reducing the danger of entrapment of any free surface film. Furthermore, experimental results showed that casting product with vortex gate leads to excellent improvement of average flexural strength and reduction of porosity and cracks defects relying on the feature of swirled flow inside the vortex gate. The ‘virtual’ experiment using a computational modeling package and the ‘physical’ experiment were found to be in reasonable agreement. 377$ 3(53867$.$$1�781.8�781�$0,1$+
format Thesis
qualification_name Master of Philosophy (M.Phil.)
qualification_level Master's degree
author Subhi, Zaid Ali
author_facet Subhi, Zaid Ali
author_sort Subhi, Zaid Ali
title The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
title_short The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
title_full The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
title_fullStr The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
title_full_unstemmed The effects of vortex gate design on mechanical strength of thin section casting of LM 25 (Al---7Si-0.3Mg) aluminum casting alloy
title_sort effects of vortex gate design on mechanical strength of thin section casting of lm 25 (al---7si-0.3mg) aluminum casting alloy
granting_institution Universiti Tun Hussein Onn Malaysia
granting_department Fakulti Kejuruteraan Mekanikal dan Pembuatan
publishDate 2012
url http://eprints.uthm.edu.my/2472/1/24p%20ZAID%20ALI%20SUBHI.pdf
_version_ 1747830960745873408